Abstract

Rapid urbanization has increased carbon emissions and solid waste generation, such as waste glass and steel slag, posing significant environmental challenges. This study investigates the combined use of waste glass powder (WGP) and Ca-rich steel slag as precursors for alkali-activated materials (AAMs), aiming to enhance performance while reducing environmental impact. In Part I, the activation behaviour of 100% WGP under different grinding methods and NaOH molarities was investigated. Ball-milled WGP, characterized by fine and rounded particles, achieved a significantly higher compressive strength than knife-milled WGP. Among the activator concentrations, 4M NaOH exhibited the most balanced performance, providing higher early strength and comparable 28-day strength to 8M NaOH. Although WGP offers promising reactivity, its long setting time restricts application. To overcome this limitation, Part II explored partial replacement of WGP with 10–50% steel slag obtained either from the primary steelmaking process (primary slag, PS) or from both primary and secondary refining processes (mixed slag, MS). The findings show that incorporating either PS or MS significantly reduced the setting time of the WGP-based AAMs. Notably, adding 20% steel slag reduced the initial setting time from over 24 hours to about 70 minutes. In terms of compressive strength, WGP-based AAMs incorporated with PS outperformed those with MS. Specifically, samples containing 20% PS achieved twice the strength of those with equivalent MS content. This is mainly due to the existence of higher portlandite content in PS, which promoted the formation of C-S-H gels. In contrast, the lower strength in samples containing MS was attributed to the presence of unreacted calcite crystalline phases, which weakened the gel network. The optimal mix was identified as 20% PS and 80% WGP, which achieved a 28-day compressive strength of 42.9 MPa and an initial setting time of 66 minutes. In Part III, a life cycle assessment was conducted on the optimal mix (20% PS and 80% WGP). The results indicated that the proposed WGPbased AAM with PS significantly reduced CO2 emissions compared with ordinary Portland cement, mainly due to the avoidance of clinker production and waste reutilization. Overall, these findings highlight the potential of reusing steel slag and waste glass as effective precursors in development of AAM, contributing to sustainable resource utilization and environmental protection.

Initial

khm

Additional Information

Dissertation (M.A.) – Faculty of Engineering, Universiti Malaya, 2026.

Share

COinS