Abstract
High carbon dioxide (CO2) emissions and susceptibility to the formation of cracks in concrete motivate bio-based, carbon-utilising approaches that improve the cementitious matrix while reducing emissions. Among these, CO₂ curing offers simultaneous materials enhancement and its interaction with blue-green microalgae inside cementitious matrices remains underexplored. This dissertation investigates blue-green microalgae, specifically Arthrospira platensis, grown in Kosaric Medium (KM) as a liquid bio-admixture and evaluates its performance under conventional water-curing and CO₂-curing conditions. Along with the culturing of microalgae, the growth profile characteristics such as optical density, pH, dry weight, and calcium uptake were investigated to confirm survivability and suitability for alkaline cementitious environments. Then, casting of 50 mm mortar cubes (w/c of 0.5 and s/c of 3.75) was done with the replacement of water with the microalgae solutions at 0%, 50%, and 100%. Another batch of casting of mortar (w/c of 0.45 and s/c of 2.75) was done with the control (C) and fully microalgae solution (M) mixes. These specimens were then cured in both conventional water-curing (CW, MW) and CO₂-curing (CC, MC) conditions in a carbonation chamber. Furthermore, fresh density, flow, and compressive strength were tested at different ages of 7-, 14-, 28-, 56-, and 90-day and a pre-crack with 65–75% of ultimate load; then after 14 days of curing in water, the specimens were assessed via UPV, residual strength, crack-image analysis, and microstructural characterisation (XRD, SEM-EDS, FTIR). The results show that the water-cured mixes, half water replacement with water produced the highest strength up to 28 days, while the whole replacement had the lowest strength; whereas at later ages of 56 and 90 days, the control surpassed the microalgae mixes by ~3–5 MPa, indicating that the specimens with microalgae do not vary much compared to the control specimens. Under CO₂ curing, the control specimens developed the highest 28-day strength of higher than 60 MPa compared to the water-cured control, which produced about 45 MPa; however, the specimens with microalgae under water remained the lowest, evidencing a clear CO₂-curing benefit and a positive interaction with microalgae. The UPV increased from 7 to 28 days for all cases; however, after pre-cracking, it dropped and partially recovered upon healing. The crack image analysis quantified minimal crack restoration in CW (12.03%) and CC (12.07%), substantial in MW (64.49%), and in MC (84.61%), confirming a strong synergy between microalgae and CO₂ curing. The XRD identified typical phases (quartz, calcite, portlandite, and ettringite), and SEM-EDS revealed denser matrices in control specimens compared to increased calcite signatures and porosity with higher microalgae content, aligning the microstructure with strength and healing trends. Overall, A. platensis solution was observed to be a viable bio-admixture; when coupled with CO₂ curing, since it enhances micro-crack closure and mechanical recovery while maintaining competitive early-age strength, highlighting a practical route for precast-oriented, lower-carbon cementitious products that combine microbial mineralisation with CO₂ utilisation.
Additional Information
Dissertation (M.A.) - Faculty of Engineering, Universiti Malaya, 2026.
Recommended Citation
Zahid, Chowdhury Zubayer, "Mechanical and residual strength of cement mortar containing blue green microalgae under water and carbon dioxide curing" (2026). Student Works (2020-2029). 2029.
https://knova.um.edu.my/student_works_2020s/2029
Creative Commons License

This work is licensed under a Creative Commons Attribution-NonCommercial-No Derivative Works 4.0 International License.
Included in
Construction Engineering and Management Commons, Structural Engineering Commons, Structural Materials Commons
Initial
khm