Abstract
The aim of this study was to evaluate the effect of bleaching agents on the marginal integrity, surface roughness, and stainability of computer-aided design-computer-aided manufacturing (CAD–CAM) ceramic-reinforced composite (CRC) crown material. A total of 120 full coverage crowns and 120 plate specimens were fabricated from four CRC materials: two milled materials; Tetric CAD (Group Tetric, n=30), Shofu Block HC (Group Shofu, n=30) and two 3D-printed materials Ceramic Crown by SprintRay (Group CC, n=30) and VarseoSmile Crown Plus by Bego (Group Bego, n=30). Specimens were assigned to three groups according to bleaching protocol: control (no bleaching), at-home bleaching with 6% hydrogen peroxide (Opalescence Go), and in-office bleaching with 35% hydrogen peroxide (Opalescence Boost) (n = 10 per material × bleaching group). Crowns were cemented onto standardized 3D-printed dies using a self-adhesive resin cement (RelyX U200) under a controlled load. The marginal gap was measured at the buccal margin before and after bleaching using swept-source optical coherence tomography (SS-OCT). Average surface roughness (Sa) was evaluated on plate specimens using focus variation microscopy technique. Stainability was assessed by measuring colour change (ΔE) after bleaching and following seven days of coffee immersion using a spectrophotometer. Statistical analyses performed included Wilcoxon signed-rank tests, paired t-tests, Kruskal–Wallis tests, oneway Analysis of Variance (ANOVA), and two-way ANOVA, with significance set at p < iv 0.05. Statistically significant increases in marginal gap were observed for all materials across all protocol (p < 0.05). However, the difference was minor, ranging from approximately 0.4 to 1.6 μm, and all values remained within clinically acceptable limits (< 120 μm). The 6% hydrogen peroxide bleaching agents produced a significant increase in Sa for Group Shofu (from 0.254 ± 0.087 μm to 0.316 ± 0.080 μm; p = 0.002) and Group Bego (0.169 ± 0.041 to 0.196 ± 0.022; p < 0.001), while no significant Sa changes were observed for Group Tetric or Group CC (p > 0.05). The 35% hydrogen peroxide, in-office bleaching agent did not result in significant surface roughness changes for any material. Colour change following bleaching protocol and subsequent coffee immersion resulted in ΔE values exceeding clinical acceptability threshold of 3.3 for Group Shofu following 6% hydrogen peroxide, at-home bleaching and Group CC in the control group.
Additional Information
Thesis (PhD) – Faculty of Dentistry, Universiti Malaya, 2026.
Recommended Citation
Rosli, Siti Rosma, "The impact of bleaching agents on marginal integrity, surface roughness and stainability of CAD-CAM ceramic-reinforced crowns" (2026). Student Works (2020-2029). 2051.
https://knova.um.edu.my/student_works_2020s/2051
Creative Commons License

This work is licensed under a Creative Commons Attribution-NonCommercial-No Derivative Works 4.0 International License.
Included in
Dental Materials Commons, Polymer and Organic Materials Commons, Prosthodontics and Prosthodontology Commons
Initial
khm